Send Message

Low Cure Blended Polyester Resin For Low Gloss Outdoor HAA Powder Coatings

Basic Information
Place of Origin: China
Brand Name: KINTE
Certification: ISO14000, ISO90001, Reach, Qualicoat, ROHS
Model Number: NH6161 & NH6687
Minimum Order Quantity: 1000kg
Price: Negotiable
Packaging Details: 25Kg/PE Bag, 875Kg/Pallet, 17,500Kg/20GP
Delivery Time: 10 working days
Payment Terms: L/C, D/P, D/A, T/T
Supply Ability: 80,000 tons per year
Product Type: Dry Blending Polyester Resins Ratio: 90/10 & 96/4
Cured Type: Polyester/HAA Curing System Cured Time: 160℃×15min
Acid Number (mgKOH/g): 68~76 & 24~29 Glass Transition Temp.( ℃): ~58 & ~56
Properties: Low Temperature Cure And Low Gloss Application: For Outdoor Semi-gloss Powder Coatings
Highlight:

Low Cure Blended Polyester Resin

,

Low Gloss Blended Polyester Resin

Low Cure Blended Polyester Resin for Low Gloss Outdoor HAA Powder Coatings

 

 

Introduction

 

NH6161 and NH6687 are high and low acid value polyester resins respectively, which are used in polyester/primid (HAA) powder coating systems. Using NH6161 and NH6687 to make powder respectively and then dry mixing to make outdoor semi-gloss powder coating.

At present, powder coatings for outdoor use are usually cured with TGIC. However, due to the physiological toxicity of TGIC, it has been banned by the European Union and other places. Therefore, the use of environmentally friendly and non-toxic HAA to replace TGIC has become the trend in the powder coating industry.

With the change in people's aesthetic concept and the problem of light pollution caused by high-gloss coatings, matte powder coatings that can produce soft surface effects are more and more widely used.

Dry-blending matting method is a commonly used method for preparing matte powder coatings. This method uses different polyesters with large differences in reactivity during the curing process. Due to the difference in reactivity, the coating surface produces a microscopically rough surface to achieve a matting effect. , the gloss of 18-45 can be obtained without adding a matting aid, and the overall cost is low.

At present, the curing temperature of polyester for dry-blended matt powder coating of the HAA system is generally 180℃, and a higher curing temperature means more energy consumption. Studies have shown that for every 10°C drop in the curing temperature of the coating, about 10% of the energy can be saved.

And NH6161 and NH6687 can achieve 160 ℃ low-temperature curing so that the application field of powder coatings has been further expanded.

 

 

Basic Features

 

Low temperature curing

Llow coating gloss

Good weather resistance and leveling

Excellent mechanical properties

Good water resistance

 

 

Recommend Formulation:

 

Formulation NH6161 NH6687

XL-552

Pigments & Fillers Leveling Aegnt Benzoin
I 200 22.2 150 2.4 1.2
II 200 8.3 150 2.4

1.2

 

 

Specifications I

 

Items NH6161 NH6687
Appearance Pale yellow flake Pale yellow flake
Acid Number (mgKOH/g) 68~76 24~29
Softening Point (℃) 100~115 100~115
Glass Transition Temp. (℃) ~58 ~56
Melting Viscosity (ICI, mPa·s) 3500±1000 5200±1200
Reactivity s (180℃, 10,5% T105) 90±40 210±80
Curing Requirement 160℃×15min
Packaging PE Bags, Net Weight 25kg ± 0.1kg / bag

 

 

Specifications II

 

Extrusion Condition Two-screw Extruder 110~120℃
Speed of Revolution 500~1200rpm
Fineness of Powder <100μm
Extrude NH6161 and NH6687 respectively according to the formula, and mix and pulverize in a ratio of 1:1 to make powder.
Application Condition Electrostatic Spraying With 40~70KV
Coating Film Thickness 50~70μm
Degreased Cold-rolled Steel 0.5mm
Film Properties Gloss (60°)

≤38%

Bending (φ1mm) Pass
Adhesive (1mm, grade) 0
Pencil Hardness ≥1H
Impact (50cm) Pass

 

 

More Code

 

Code Ratio Cure Cycle Acid Value (mgKOH/g) Viscosity (mPa.s/200℃) Tg (℃) Reactivity (s/180℃) Properties
NH6083 90/10 180℃*10min 80~90 1500~3500 ~58 30-90 Fast cure resin. For one shot matt formulations.
NH6685 96/4 180℃*10min 19~24 4800~6400 ~57 220-280
NH6381 93/7 180℃*10min 47~54 3800~4800 ~60 60-120 Dry-blended for low gloss powder coatings with good mechanical properties and flow.
NH6688 96/4 180℃*15min 19~24 4800~6400 ~56 220-280
NH6161 91/9 160℃*15min 68~76 2500~4500 ~59 50-150 Low bake resins. Dry-blended for low gloss powder coatings, with good mechanical properties and flow.
NH6687 96/4 160℃*15min 24~29 4000~6500 ~56 160-260

 

 

Remarks: All the polyester resins could be customized to Non-tin (A), anti gas burners (G), tribo gun (T) and anti-blooming (F).

 

 

Company Profile:

 

Kinte Materials Science and Technology Co., Ltd. is subordinate to China Machinery Industry Corporation (a key state-owned enterprise directly managed by SASAC, ranking 284 among the world's top 500 in 2021). It is a national high-tech enterprise under China National Electric Apparatus Research Institute Co., Ltd. (Stock Code: 688128), a listed enterprise on the SSE STAR MARKET. Focusing on the R & D, production, and sales of environmentally friendly coatings (powder coatings, waterborne industrial coatings) and powder coating resins, the company is committed to improving the global market competitiveness of China's environmentally friendly coating industry. Now it has become the leader and promoter in China’s technological development of environmentally friendly coatings as well as polyester resins for powder coatings!

Low Cure Blended Polyester Resin For Low Gloss Outdoor HAA Powder Coatings 0

 

We have gained ISO9001 and ISO14000, ISO18001, RoHS, UL certification and QUALICOAT Certificate. Due to the excellent and stable quality, our products always enjoy high reputation at home and oversea, and were sold to more than 30 countries.

Low Cure Blended Polyester Resin For Low Gloss Outdoor HAA Powder Coatings 1

 

 

Polyester resin branch was founded in 2000, now there are two factories (DongGuan factory and TaiXing Factory) with annual production capacity over 80,000 tons, and the annual production capacity reached 120000 tons by the end of 2020, opening the road to global diversified development. Our clients include many top-tier powder manufacturers in the world such as AKZO, PPG, TIGER, PROTECH, NIPPON, OXYPLAST, JOTUN, SHERWIN, VALSPAR, SINTERPLAST, etc.

Low Cure Blended Polyester Resin For Low Gloss Outdoor HAA Powder Coatings 2

 

We unremittingly stick at the business principle of “Quality is the life, adhere to first-class technology, first-class quality, first-class cost and first-class brand”. We would like to provide a complete set of services and solutions for both domestic and abroad customers and would like to go forward to brilliant future with you together.

Low Cure Blended Polyester Resin For Low Gloss Outdoor HAA Powder Coatings 3

Contact Details
Kintechem

Phone Number : +8613590248009

WhatsApp : +8618620810858